ABD Composites is laminate analysis software that runs in your browser. Build a layup, apply a load, and the ABD matrix, ply stresses and failure margins update as you type. There is no install, no license server and no spreadsheet to pass around.

  • Runs in the browser
  • Metric and imperial units
app.abdcomposites.com
CLIP loops
Type a layup code. The stack fills in and rotates.

What the Software Computes

The tools follow the order of a design: ply, laminate, load, failure, then the part. Each one hands its result to the next, so a ply built from fiber and resin data goes straight into a laminate.

LaminateCLT

You enter

Stacking sequence or layup code, ply material and thickness

You get

ABD matrix; membrane and flexural engineering constants; CTE and CME; carpet plots across 0°, ±45° and 90° mixes

Docs
CLT Theory
app.abdcomposites.com
CLIP loops
Edit the layup. The ABD matrix and the deformed plate update, then First Ply Failure shows the failing ply and its stress through the thickness.

Results show in metric or imperial units, and you can pick the unit of each quantity on its own. The docs give the theory and a how-to for every tool.

Who Uses It

It is built for composites and structural engineers who run laminate trade studies: in aerospace, space and defense, on drones, boats and race cars, on wind blades, and at composite part manufacturers. The usual jobs are comparing a handful of layups against a stiffness or strength target before anyone builds an FE model, checking a hand calculation or an FE result against CLT, and sizing a panel, a tube or a bolted joint for a quote.

That work often sits in a spreadsheet, a Python script or an old desktop program installed on one machine. In ABD Composites your materials and laminates are saved to your account and open on any computer you sign in from.

Worked Example: Ply Stresses in a [±45]s Laminate

A [45/−45]s laminate of T300/5208 carbon/epoxy, four plies of 0.125 mm, carries Nx = 100 N/mm of tension and no other load. What stresses does each ply see in its fiber axes, and does it hold?

Ply propertyValue
E1181000 MPa
E210300 MPa
G127170 MPa
ν120.28
S1t / S1c1500 / 1500 MPa
S2t / S2c40 / 246 MPa
S1268 MPa
ResultValue
A11 = A2228328.9 N/mm
A1221158.9 N/mm
A6623295.4 N/mm
εx, εy7984, −5963 µε
σ1, σ2186.6, 13.38 MPa
τ12±100 MPa
Tsai-Wu SF0.6161
First-ply failure61.6 N/mm

The stack is symmetric and balanced, so B = 0 and A16 = A26 = 0. The fibers carry 186.6 MPa, about 12% of their strength. The shear in the fiber axes is what fails the plies: 100 MPa against S12 = 68 MPa. Tsai-Wu puts first-ply failure at 61.6 N/mm, well under the 100 N/mm applied.

-150-5050150250Stress (MPa)SF = 102468Tsai-Wu SF0153045607590Ply angle θ (°)
σ1σ2τ12Tsai-Wu SF, +θ ply
The same laminate with the ply angle swept from 0 to 90°. Toward 0° the fibers take the load and the Tsai-Wu safety factor climbs to 7.5. Toward 90° σ2 takes over and it falls to 0.2.

Read the full [±45]s worked example, which goes step by step from the A matrix to the safety factor and lets you sweep the ply angle from 0 to 90°. There are more in all worked examples, from micromechanics to bolted joints.

Reference: Jones, R.M., Mechanics of Composite Materials, 2nd Ed., Taylor & Francis, 1999.

How the Results Are Checked

Every expected value in the calculation engine's tests comes from outside the code: a textbook worked example or an independent implementation of the same theory. The worked examples go further. They set predictions next to published test data, including the cases where the defaults miss.

Open holes and bolted joints, IM7-8552

Safe side: prediction below testPrediction above testOpen hole, OHT1, Tool defaults: test 252 MPa, predicted 263 MPa (+4.3%)Open hole, OHT2, Tool defaults: test 373 MPa, predicted 302 MPa (−19.0%)Open hole, OHT2, d0 calibrated on one test: test 373 MPa, predicted 387 MPa (+3.8%)Open hole, OHT3, Tool defaults: test 439 MPa, predicted 313 MPa (−28.7%)Open hole, OHT3, d0 calibrated on one test: test 439 MPa, predicted 398 MPa (−9.3%)Open hole, OHT4, Tool defaults: test 247 MPa, predicted 231 MPa (−6.6%)Open hole, OHT5, Tool defaults: test 367 MPa, predicted 272 MPa (−25.8%)Open hole, OHT5, d0 calibrated on one test: test 367 MPa, predicted 367 MPa (+0.1%)Open hole, OHT6, Tool defaults: test 376 MPa, predicted 282 MPa (−24.9%)Open hole, OHT6, d0 calibrated on one test: test 376 MPa, predicted 378 MPa (+0.6%)Open hole, OHT7, Tool defaults: test 261 MPa, predicted 208 MPa (−20.2%)Open hole, OHT7, d0 calibrated on one test: test 261 MPa, predicted 298 MPa (+14.3%)Open hole, OHT8, Tool defaults: test 345 MPa, predicted 251 MPa (−27.1%)Open hole, OHT8, d0 calibrated on one test: test 345 MPa, predicted 350 MPa (+1.6%)Open hole, OHT9, Tool defaults: test 374 MPa, predicted 260 MPa (−30.4%)Open hole, OHT9, d0 calibrated on one test: test 374 MPa, predicted 361 MPa (−3.4%)Open hole, C12-d2, Tool defaults: test 556 MPa, predicted 403 MPa (−27.5%)Open hole, C12-d2, d0 calibrated on one test: test 556 MPa, predicted 459 MPa (−17.4%)Open hole, C12-d4, Tool defaults: test 481 MPa, predicted 353 MPa (−26.6%)Open hole, C12-d4, d0 calibrated on one test: test 481 MPa, predicted 425 MPa (−11.6%)Open hole, G-3.175, Tool defaults: test 478 MPa, predicted 366 MPa (−23.4%)Open hole, G-3.175, d0 calibrated on one test: test 478 MPa, predicted 435 MPa (−9.0%)Open hole, G-6.35, Tool defaults: test 433 MPa, predicted 303 MPa (−30.0%)Open hole, G-6.35, d0 calibrated on one test: test 433 MPa, predicted 390 MPa (−9.9%)Open hole, G-12.7, Tool defaults: test 374 MPa, predicted 237 MPa (−36.6%)Open hole, G-12.7, d0 calibrated on one test: test 374 MPa, predicted 337 MPa (−9.9%)Open hole, G-25.4, Tool defaults: test 331 MPa, predicted 198 MPa (−40.2%)Open hole, G-25.4, d0 calibrated on one test: test 331 MPa, predicted 265 MPa (−19.9%)Bolted joint, DSBFB, Tool defaults: test 695 MPa, predicted 539 MPa (−22.5%)Bolted joint, DSBFB, Characteristic curve: test 695 MPa, predicted 645 MPa (−7.2%)Bolted joint, DSSFB, Tool defaults: test 702 MPa, predicted 613 MPa (−12.7%)Bolted joint, DSSFB, Characteristic curve: test 702 MPa, predicted 688 MPa (−2.0%)Bolted joint, DSTFB, Tool defaults: test 527 MPa, predicted 533 MPa (+1.2%)Bolted joint, DSTFB, Characteristic curve: test 527 MPa, predicted 520 MPa (−1.2%)Bolted joint, DSBFP, Tool defaults: test 706 MPa, predicted 539 MPa (−23.7%)Bolted joint, DSBFP, Characteristic curve: test 706 MPa, predicted 610 MPa (−13.6%)Bolted joint, DSSFP, Tool defaults: test 699 MPa, predicted 613 MPa (−12.4%)Bolted joint, DSSFP, Characteristic curve: test 699 MPa, predicted 635 MPa (−9.2%)Bolted joint, DSTFP, Tool defaults: test 461 MPa, predicted 533 MPa (+15.7%)Bolted joint, DSTFP, Characteristic curve: test 461 MPa, predicted 520 MPa (+12.9%)200300400500600700200300400500600700Test strength (MPa)Predicted strength (MPa)
  • Open hole, tool defaults
  • Open hole, d0 calibrated on one test
  • Bolted joint, tool defaults
  • Bolted joint, characteristic curve
  • Safe side: prediction below test

Each point is one published test. On the dashed line the prediction equals the test. Points in the shaded area below it are on the safe side: the tool predicts less strength than the test showed. Open-hole tension: Camanho and Lambert (2006) and Camanho et al. (2012), which also tabulates Green et al. Bolted joints: Camanho and Lambert (2006). The bolted joint page also runs the open-hole d0 on the joints, which overpredicts by 49 to 60%; those points sit off this scale.

Laminate Results Against Outside References

Lab tests: strength

Validation: failure loads of coupons, tubes, beams and joints, compared with published test programs. Where the app has several failure criteria, a case scores by Puck. The other criteria show in its row.

Cases
150 cases from 5 sources, 1322 compared numbers
Within 10 %
64 of 150
Median error
7.91 %, known gaps left out
Bias and scatter
−1.45 % on average, ±10.2 % scatter (1 SD)
Known gaps
46, see the list

Published solutions

Verification: the same inputs run against worked examples, tables and closed-form answers printed in textbooks, NASA reports and journal papers.

Cases
15 cases from 4 sources, 55 compared numbers
Within 1 %
11 of 15
Median error
0.0092 %
Largest error
1.27 %
Known gaps
None

Finite element models

Verification: a plane-stress finite element model of the same problem, solved in an open-source code. Each model runs on two meshes.

No finite element model is listed for lamina, laminate and failure yet.

ABD Composites runs no tests of its own. Each measured value comes from a published test program.

See every case, its source and how to reproduce it

Frequently Asked Questions

Analyze Your Own Laminate